How Do I Make A Electrolysis Machine To Use For Welding

Meaningful discussion outside of the potato gun realm. Projects, theories, current events.
User avatar
ramses
Staff Sergeant 2
Staff Sergeant 2
United States of America
Posts: 1679
Joined: Thu May 29, 2008 6:50 pm

NOOO!!!!!!!!!

Do NOT use galvanized in a KOH solution. The KOH will react with the zinc coating, creating hydrogen ( in a non-stoich. ratio) and exposing the normal steel.

Also, in chlorate cells (essentially the same thing, with more strict requirements and less current moving), a 5v computer PSU is often used. A cheap one I recently got rid of was rated for over 25 amps at 5v! Should you choose this option, you should use all the ground wires for your ground, and all the +5v wires for the +5. Don't try to dump 25 amps through a single wire, as the insulation will most likely burn off.

http://www.instructables.com/id/ATX--%3 ... onversion/
POLAND_SPUD wrote:even if there was no link I'd know it's a bot because of female name :D
User avatar
rp181
Sergeant
Sergeant
Posts: 1090
Joined: Thu Dec 13, 2007 8:47 pm
Contact:

Actually, galvanized electrodes can be used.
When I used some, the zinc reacts off, but the remaining steel works fine. Potassium hydroxide also cleans the electrodes, oxidation won't be a problem, but the solution has to replaced every once in a while.
Post Reply

Create an account or sign in to join the discussion

You need to be a member in order to post a reply

Create an account

Not a member? register to join our community
Members can start their own topics & subscribe to topics
It’s free and only takes a minute

Register

Sign in

  • Similar Topics
    Replies
    Views
    Last post